Home > News > Technical conditions for gold extraction by electrowinning

Technical conditions for gold extraction by electrowinning

2023-12-28
Electrodeposition technology in recent years developed a new technology to get pure gold from gold-rich silver solution. The electrodeposition tank uses stainless steel as the anode and steel wool as the cathode. After the direct current is applied, about 80% of pure gold can be obtained on the cathode. The distance between the poles is 35 mm, the voltage in the tank is 3 to 4.5 volts, the cathode current density is 15 to 20 amps/m 2 , and the flow rate of the electrowinning fluid is 1.5 to 2 liters/min. Electrodeposition is carried out at room temperature. The electro-product cycle is 24 to 48 hours, and the electro-hydration solution (for a groove volume of 0.036 m 3 ) can be treated at 800 to 1000 liters at a time. The electric volume rate can reach more than 99%.
A steel wire (steel cotton consumption of 0.89 g steel/two gold) with a certain amount of gold is raised by a cathode, and immersed in 1:1 industrial hydrochloric acid to remove stainless steel wool and its impurities. After drying the treated powder was placed in a crucible, adding 8 to 25% of borax, 5 to 30% of sodium carbonate, 5 to 25% silica, adding an appropriate amount of saltpetre melting at 1200 deg.] C ~ 15 In 25 minutes, a gold ingot having a purity of 92 to 93% can be obtained.
Product Categories

Home

Product

Phone

About Us

Inquiry

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

Send